碲硒锌镉单晶体的垂直布里奇曼法生长与性能研究
DOI:
CSTR:
作者:
作者单位:

电子科技大学

作者简介:

通讯作者:

中图分类号:

O782

基金项目:

国家自然科学(62374025,U20A20145)


Growth and properties of single crystals of cadmium zinc telluride selenide by vertical Bridgman method
Author:
Affiliation:

School of Materials and Energy,University of Electronic Science and Technology of China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    碲锌镉(CdZnTe)是目前最重要的室温半导体核辐射探测器材料。而在CdZnTe晶格中以Se替位部分Te得到碲硒锌镉(CdZnTeSe),将使得晶格中离子键的成分增加,从而提高晶体的硬度,降低Cd空位和Te夹杂物缺陷浓度,提升材料质量。为了获得适宜于核辐射探测器制备的CdZnTeSe晶体,本工作研究了富Te条件下CdZnTeSe晶体的垂直布里奇曼法生长,成功制备出直径21 mm、长度超过70 mm的Cd0.9Zn0.1Te0.97Se0.03单晶锭。所得Cd0.9Zn0.1Te0.97Se0.03晶体的(1 1 0)面X射线衍射摇摆半峰宽达到0.104°,而Te夹杂相的尺寸<5 μm,表明晶体具有良好结晶性。Cd0.9Zn0.1Te0.97Se0.03晶锭尾部的能带隙和红外透过率均低于晶锭的头部和中部,可归因于Cd0.9Zn0.1Te0.97Se0.03在垂直布里奇曼法生长过程中存在着潜热释放不足导致的晶体后续生长阶段的结晶性下降。而CdZnTeSe晶锭的头部和中部的电学性能指标达到了室温核辐射探测器制备要求。

    Abstract:

    Cadmium zinc telluride (CdZnTe) is the most crucial room-temperature semiconductor nuclear radiation detector material. The substitution of some Te with Se in the CdZnTe lattice to obtain cadmium zinc telluride selenide (CdZnTeSe) will lead to an increase in the composition of ionic bonds in the lattice, which will improve the hardness of the crystal, reduce the concentration of Cd vacancies and Te inclusions defects, and enhance the quality of the material. In order to obtain CdZnTeSe crystals suitable for the preparation of nuclear radiation detectors, in this work, the growth of CdZnTeSe crystals under Te-rich conditions was investigated by the vertical Bridgman method, and Cd0.9Zn0.1Te0.97Se0.03 single-crystal ingots with a diameter of 21 mm and a length of more than 70 mm were successfully prepared. The obtained Cd0.9Zn0.1Te0.97Se0.03 crystals have an X-ray diffraction wobble half-peak width of 0.104° in the (1 1 0) plane, whereas the size of the Te intercalation phase is <5 μm, which indicates that the crystals have good crystallinity. The energy band gap and IR transmittance of Cd0.9Zn0.1Te0.97Se0.03 ingot tails are lower than that of the head and middle of the ingot, which can be attributed to the decrease of crystallinity in the subsequent growth stages of the crystals due to the insufficient release of latent heat during the growth of Cd0.9Zn0.1Te0.97Se0.03 by the vertical Bridgman method. Moreover, the electrical performance indexes of the head and middle of the CdZnTeSe ingots meet the requirements for preparing room-temperature radiation detectors.

    参考文献
    相似文献
    引证文献
引用本文
分享
相关视频

文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2023-10-27
  • 最后修改日期:2023-10-27
  • 录用日期:2023-11-01
  • 在线发布日期:
  • 出版日期:
文章二维码