磁控溅射氮化硅薄膜及微环谐振器的超高真空退火研究
DOI:
CSTR:
作者:
作者单位:

上海大学 微电子学院

作者简介:

通讯作者:

中图分类号:

TN256

基金项目:

国家重点研发计划项目(2024YFA1209100);传感器技术全国重点实验室(SKT2510);上海市科研计划项目(25TS1410400、24JD1401800);上海市汽车智能网联交互芯片与系统重点实验室项目;国家自然科学(62575166).,国家自然科学基金项目(面上项目,重点项目,重大项目)


Study on Ultra-High Vacuum Annealing of Magnetron-Sputtered Silicon Nitride Films and Microresonators
Author:
Affiliation:

School of Microelectronics,Shanghai University

Fund Project:

the National Key Research and Development Program of China under Grant 2024YFA1209100, Foundation of the State Key Laboratory of Transducer Technology (No. SKT2510), Research Program of Shanghai under Grant 25TS1410400 and 24JD1401800, Shanghai Key Laboratory of Chips and Systems for Intelligent Connected Vehicle, the National Natural Science Foundation of China (62575166).

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    室温磁控溅射制备的氮化硅(SiN)薄膜具有低氢含量和低温工艺兼容性等优势,但仍需通过后退火处理降低由结构缺陷引起的光散射损耗。本文系统研究超高真空(UHV)退火对室温溅射SiN薄膜及微环谐振器性能的影响。采用X射线光电子能谱、傅里叶变换红外光谱、原子力显微镜、椭圆偏振光谱仪及透射谱测试表征400、600、800 ℃退火后薄膜成分、化学键合状态、表面形貌、折射率以及器件本征品质因子(Qi)与传播损耗。结果表明:400℃退火后器件性能最佳,Qi由2.9×104提升至3.4×104,传播损耗由9.6 dB/cm降至8.1 dB/cm;继续升高退火温度,器件性能明显下降,800 ℃时虽有所恢复,但仍低于未退火水平。

    Abstract:

    Silicon nitride (SiN) films deposited by room-temperature magnetron sputtering offer low hydrogen content and compatibility with low-temperature processing, but post-annealing is still required to reduce optical scattering loss caused by structural defects. In this work, the effects of ultra-high vacuum (UHV) annealing on room-temperature sputtered SiN films and microresonators were systematically investigated. Material properties including film composition, bonding configuration, surface morphology, and refractive index were characterized using X-ray photoelectron spectroscopy, Fourier transform infrared spectroscopy, atomic force microscopy, and ellipsometry after annealing at 400, 600, and 800 °C. Meanwhile, optical transmission measurements were performed to extract the intrinsic quality factor (Qi) and propagation loss of the devices. The results indicate that the device performance was optimal after annealing at 400 °C, where the Qi increased from 2.9×104 to 3.4×104 and the propagation loss decreased from 9.6 to 8.1 dB/cm. With a further increase in annealing temperature, the device performance degraded significantly. Although partial recovery was observed at 800 °C, the performance remained inferior to that of the as-deposited device.

    参考文献
    相似文献
    引证文献
引用本文
分享
相关视频

文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2026-04-19
  • 最后修改日期:2026-04-19
  • 录用日期:2026-05-15
  • 在线发布日期:
  • 出版日期:
文章二维码